产品参数
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 |
吸水率 | | ASTM D570 | 0.2 | % |
流动系数 | 300℃ 1.2kg | ASTM D1238 | 10 | g/10min |
成型收缩率(-) | Parallel | ASTM D955 | 0.5-0.7 | % |
成型收缩率(-) | across | ASTM D955 | 0.5-0.7 | % |
比重 | | ASTM D792 | 1.20 |
曲折率 | | ASTM D542 | 1.585 |
洛氏硬度 | | ASTM D785 | 77 | M |
Izod缺口冲击强度(-) | 1/4″ | ASTM D256 | 15 | Kg.cm/cm |
Izod缺口冲击强度(-) | 1/8″ | ASTM D256 | 87 | Kg.cm/cm |
弯曲强度 | 23℃ | ASTM D790 | 920 | kg/cm2 |
延伸率(降伏点) | 23℃ | ASTM D638 | 6 | % |
延伸率(破断点) | 23℃ | ASTM D638 | 110 | % |
引张强度 | 23℃ | ASTM D638 | 630 | kg/cm2 |
弯曲模量 | 23℃ | ASTM D790 | 24000 | kg/cm2 |
压缩强度 | | ASTM D695 | 780 | kg/cm2 |
介电常数(-) | 60Hz | ASTM D150 | 2.95 |
介电常数(-) | 106Hz | ASTM D150 | 2.9 |
体积电阻率 | | ASTM D257 | 3 | ×1016Ω?cm |
耐电弧性 | | ASTM D495 | 110 | sec |
绝缘破坏强度 | 1.6mm | ASTM D149 | 30 | KV/mm |
软化点温度 | | ASTM D1525 | 150 | ℃ |
热传导率 | | ASTM C177 | 0.2 | W/m℃ |
阻燃性 | 3.0mm | UL94 | V-2 |
热变形温度(-) | 4.6kg/cm2 | ASTM D648 | 136 | ℃ |
热变形温度(-) | 18.6kg/cm2 | ASTM D648 | 125 | ℃ |
线膨胀系数 | 40-100℃ | ASTM D696 | 6-8 | ×105cm/cm/℃ |
浊度 | | ASTM D1003 | <0.8 | % |
全光穿透率 | 3mm | ASTM D1003 | 89 | % |
特性:阻燃,一般射出成型。
产品加工条件:
1)于120°C下烘料约4小时
2)射出套筒温度介于230~320°C
3)模温为70~120°C
4)在射出周期中勿将热融胶长期停留在加热管中
长期供应PC韩国LG-DOW1201-10、1201-15、201-10、201-8、201-15、201-22、301V-10、303-10台湾奇美PC-110、PC-122、PC-115、PC-175、PC-110U、PC-122U、PC-110V原厂原包,价格优惠,欢迎来电洽谈!