主要用途:广泛用于冶金、建材、化工、石油、机械制造、硅酸盐、动力等工业领域
通用粘土砖理化指标:
项 目 | 指 标 | |
N-1 | N-2a | N-2b | N-3a | N-3b | N-4 | N-5 | N-6 |
耐火度,℃ | ≥1750 | ≥1730 | ≥1730 | ≥1710 | ≥1710 | ≥1690 | ≥1670 | ≥1580 |
荷重软化开始温度,℃,[0.2MPa×0.6%] | ≥1400 | ≥1350 | | ≥1320 | | ≥1300 | | |
重烧线变化率,% | 1400℃×2h | +0.1 -0.4 | +0.1 -0.5 | +0.2 -0.5 | | | | | |
1350℃×2h | | | | +0.2 -0.5 | +0.2 -0.5 | +0.2 -0.5 | +0.2 -0.5 | |
显气孔率 | ≤22 | ≤26 | ≤24 | ≤24 | ≤26 | ≤24 | ≤26 | ≤28 |
常温耐压强度,MPa | ≥30.0 | ≥20.0 | ≥25.0 | ≥20.0 | ≥15.0 | ≥20.0 | ≥15.0 | ≥15.0 |