性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
基本性能 | 密度 | --- | ASTM D-792 | 1.42 | --- |
物理性能 | 吸水量 | 24hrs浸泡+73?H(+23℃) | ASTM D-570 | 0.25 | % |
吸水量 | Equil.50%R.h.+73?H(+23℃) | ASTM D-570 | 0.22 | % | |
吸水量 | 浸泡均衡点+73?H(+23℃) | ASTM D-570 | 0.90 | % | |
扩散因数 | +73?H(+23℃)106Hz | ASTM D-150 | 0.005 | --- | |
机械性能 | 无切口冲击程度 | +23℃ | ASTM D-256 | 1280 | j/m |
压缩应力 | +73?H@10% Def. | ASTM D-695 | 18.0 | MPsi | |
压缩应力 | +23℃@10% Def. | ASTM D-695 | 124 | MPa | |
负载下之变形 | 2000psi@+122?H(14Mpa@50℃) | ASTM D-621 | 0.5 | % | |
弯曲疲劳忍耐限度 | +73?H | ASTM D-671 | 4.5 | MPsi | |
弯曲疲劳忍耐限度 | +23℃ | ASTM D-671 | 31.0 | MPa | |
IZOD冲击强度 | -40?H | ASTM D-256 | 1.2 | ft.lb/in | |
IZOD冲击强度 | 40℃ | ASTM D-256 | 64.1 | j/m | |
IZOD冲击强度 | +73?H | ASTM D-256 | 1.4 | ft.lb/in | |
IZOD冲击强度 | +23℃ | ASTM D-256 | 74.7 | j/m | |
拉力冲击抵抗力 | +73?H | ASTM D-1822 | 100 | ft.lb/in2 | |
拉力冲击抵抗力 | +23℃ | ASTM D-1822 | 200 | kj/m2 | |
无切口冲击程度 | +73?H | ASTM D-256 | 24 | ft.lb/in | |
断裂时之拉力伸张度 | -68?H(-55℃) | ASTM D-638 | 13 | % | |
断裂时之拉力伸张度 | +73?H(+23℃) | ASTM D-638 | 40 | % | |
断裂时之拉力伸张度 | +158?H(+70℃) | ASTM D-638 | 220 | % | |
断裂时之拉力伸张度 | +212?H(+100℃) | ASTM D-638 | >260 | % | |
断裂时之拉力伸张度 | +250?H(+122℃) | ASTM D-638 | >260 | % | |
伸张强度 | -68?H | ASTM D-638 | 14.7 | MPsi | |
伸张强度 | -55℃ | ASTM D-638 | 101 | MPa | |
伸张强度 | +73?H | ASTM D-638 | 10.0 | MPsi | |
伸张强度 | +23℃ | ASTM D-638 | 68.9 | MPa | |
伸张强度 | +158?H | ASTM D-638 | 6.9 | MPsi | |
伸张强度 | +70℃ | ASTM D-638 | 47.5 | MPa | |
伸张强度 | +212?H | ASTM D-638 | 5.2 | MPsi | |
伸张强度 | +100℃ | ASTM D-638 | 35.9 | MPa | |
伸张强度 | +250?H | ASTM D-638 | 3.8 | MPsi | |
伸张强度 | +122℃ | ASTM D-638 | 26.2 | MPa | |
弹性系数 | +73?H | ASTM D-638 | 450 | MPsi | |
弹性系数 | +23℃ | ASTM D-638 | 3100 | MPa | |
剪力 | +73?H | ASTM D-732 | 9.5 | MPsi | |
剪力 | +23℃ | ASTM D-732 | 65.5 | MPa | |
挠曲系数 | -68?H | 在25℃下 | 570 | MPsi | |
挠曲系数 | -55℃ | 在25℃下 | 3930 | MPa | |
挠曲系数 | +73?H | 在25℃下 | 410 | MPsi | |
挠曲系数 | +23℃ | 在25℃下 | 2830 | MPa | |
挠曲系数 | +158?H | 在25℃下 | 230 | MPsi | |
挠曲系数 | +70℃ | 在25℃下 | 1585 | MPa | |
挠曲系数 | +212?H | 在25℃下 | 135 | MPsi | |
挠曲系数 | +100℃ | 在25℃下 | 90 | MPsi | |
挠曲系数 | +122℃ | 在25℃下 | 620 | MPa | |
弯曲降服强度 | +73?H | ASTM D-790 | 14.1 | MPsi | |
弯曲降服强度 | +23℃ | ASTM D-790 | 97.2 | MPa | |
压缩应力 | +73?H@1% Def. | ASTM D-695 | 5.2 | MPsi | |
压缩应力 | +23℃@1%Def. | ASTM D-695 | 35.9 | MPa | |
洛氏硬度 | --- | ASTM D-785 | M94,R120 | --- | |
摩擦系数 | +73?H(+23℃)静态 | ThrustWasherTest3 | 0.20 | --- | |
摩擦系数 | +73?H(+23℃)动态 | ThrustWasherTest3 | 0.35 | --- | |
电气性能 | 电弧抵抗力 | 120mil(3.1mm) | ASTM D-495 | 220no tracking | Sec. |
绝缘强度 | Short Time,90 mils | ASTM D-149 | 500 | V/mil | |
绝缘强度 | Short Time,2.3mm | ASTM D-149 | 19.7 | MV/m | |
绝缘系数 | +73?H(+23℃)102to106Hz | ASTM D-150 | 3.7 | --- | |
电阻系数 | +73?H(+23℃)0.2%H2O | ASTM D-257 | 1015 | ohm-cm | |
热 性 能 | 热传导系数 | W/mk | --- | 0.37 | --- |
线性热膨胀系数 | +60 to +104℃ | ASTM D-696 | 13.7 | 10-5m/m.℃ | |
线性热膨胀系数 | +220 to +300?H | ASTM D-696 | 8.3 | 10-5in/in.?H | |
线性热膨胀系数 | +104 to +150℃ | ASTM D-696 | 14.9 | 10-5m/m.℃ | |
热传导系数 | BTU-in/hr | --- | 2.6 | --- | |
熔点 | --- | ASTM D-2133 | 347 | ?H | |
熔点 | --- | ASTM D-2133 | 175 | ℃ | |
线性热膨胀系数 | -40 to +85?H | ASTM D-696 | 5.8 | 10-5in/in.?H | |
线性热膨胀系数 | -40 to +29℃ | ASTM D-696 | 10.4 | 10-5m/m.℃ | |
线性热膨胀系数 | +85 to +140?H | ASTM D-696 | 6.8 | 10-5in/in.?H | |
线性热膨胀系数 | +29 to +60℃ | ASTM D-696 | 12.2 | 10-5m/m.℃ | |
线性热膨胀系数 | +140 to +220?H | ASTM D-696 | 7.6 | 10-5in/in.?H | |
热变形温度 | 0.5MPa | ASTM D-648 | 172 | ℃ | |
热变形温度 | 1.8MPa | ASTM D-648 | 136 | ℃ | |
热变形温度 | 66psi | ASTM D-648 | 342 | ?H | |
热变形温度 | 264psi | ASTM D-648 | 277 | ?H | |
可燃烧性 | --- | UL-94 | 94HB | --- |
1.供应POM,SX-35日本宝理消音齿轮;2.供应POM,M25-44,M25S日本宝理高粘性;
3.供应POM,M90-44,M270-44,M270S日本宝理高流动性;
4.供应POM,AW-01,NW-02,SW-01日本宝理高滑动性;
5.供应POM,GH-25,GR-20日本宝理玻纤增强;GM-20;GB-25;
6.供应POM,M90-48,M270-48日本宝理防静电;
7.供应POM,M270-45,M90-45日本宝理耐候级,M270-35/36,M90-35/36,M25-45,M25-35;
8.供应POM日本宝理M270,M90,M25-34,WR90Z,WR25HT,UV25Z,UV90Z,UV270Z,M140-35;
9.供应POM日本杜邦100P,DE-20242, DE9422-NC.
10.供应POM,FX-11J泰国三菱耐磨级;
供应POM,FG2025泰国三菱25%玻纤增强耐磨级;
11.供应POM,500P,500T美国杜邦中粘低磨耗;
12.供应POM,100P,200P美国杜邦高粘高应力耐磨级;
13.供应POM,100ST,100T美国杜邦高粘高负载超强韧性;
14.供应POM,900P,911P美国杜邦低粘高流动性;
15.供应POM,500CL,500AL美国杜邦中粘高耐磨;
16.供应POM,100AF,500AF美国杜邦铁氟龙高耐磨(20%TEFLON3);
供应POM,525GR,570,510GR美国杜邦玻纤增强耐磨级(25%,20%,10%);
17.供应POM,588P美国杜邦,23P,45P,100,107,390PM,511P,500(BK602);
供应POM美国泰科纳UV90Z,M90SW,M90UV,M270UV,UV25Z,M25UV,LM90Z,WR25Z,M90-45H;
18.供应POM,527UV,107UV,127UV美国杜邦耐高温抗紫外线;
19.供应POM新加坡杜邦耐磨级500CL,100P,500P;
20.供应POM欧盟杜邦107UV(耐高温抗紫外线);500P,100ST;
21.供应POM德国巴斯夫N2320-003,N2200,H2320-006,H4320-Q600,S2320-003,W2320-003.
22.供应POM德国赫斯特C27021,C52021,C9021,C2521,C13021;
23.供应POM杜邦-旭化成(张家港)通用级4520,7520;
24.供应POM台丽钢一般级FM130,FM090,FM270,FM350,FM450,FM550;
25.供应POM南通宝泰菱F20-02,F20-30,M90-44;
26.供应POM,500P,100P;588P深圳杜邦;
27.供应POM,FU2025韩国工程耐候级;
供应POM,FG2015,FG2025韩国工程玻纤增强;
性质:POM是结晶性热可塑性塑料,具明显熔点165-175℃,性质最接近金属,一般称其为塑钢。
优点:1、具高机械强度和刚性;
2、的疲劳强度;
3、境抵抗性、耐有机溶剂性佳;
4、反覆冲击性强;
5、广泛的使用温度范围(-40℃~120℃);
6、良好的电气性质;
7、复原性良好;
8、具自已润滑性、耐磨性良好;9、尺寸安定性优。
用途:电子电器:洗衣机,果汁机定时器等组件;
汽车:车把,电动窗等零件;机械零件,齿轮,把手,螺杆,玩具等;
分类:玻纤/碳纤增强POM,防火POM,抗紫外线耐候POM,加铁氟龙POM,防静电/导电POM;