PP台湾台化K8005 物性认证数据表
数据提供企业:
性能项目 | 测试条件 | 测试方法 | 数值/描述 | 单位 |
机械性能 | 拉伸强度(引张强度) | | ASTM D638/ISO 527 | 260 | kg/cm²(MPa)[Lb/in2] |
断裂伸长率 | | ASTM D638/ISO 527 | >200 | % |
拉伸模量 | | ASTM D638/ISO 527 | | kg/cm²(MPa)[Lb/in2] |
拉伸屈服伸长率(延伸率) | | ASTM D638/ISO 527 | | % |
拉伸断裂伸长率(延伸率) | | ASTM D638/ISO 527 | | % |
弯曲模量(弯曲弹性率) | | ASTM D790/ISO 178 | 11500 | kg/cm²(MPa)[Lb/in2] |
弯曲强度 | | ASTM D790/ISO 178 | | kg/cm²(MPa)[Lb/in2] |
洛氏硬度 | | ASTM D785 | 85 | kg·cm/cm(J/M)ft·lb/in |
IZOD 冲击强度 | 1/4" 23℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
1/4" -30℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
1/8" 23℃ | ASTM D256/ISO 179 | N.B | kg·cm/cm(J/M)ft·lb/in |
1/8" -30℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
Charpy冲击强度 | 23℃ (缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
-30℃(缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
23℃(无缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
-30℃(无缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
物性性能 | 比重(密度) | | ASTM D792/ISO 1183 | 0.9 | |
成型收缩率 | | ASTM D955 | 1.4~1.8 | % |
熔融指数(流动系数) | 200℃/5kg | ASTM D1238/ISO 1133 | | g/10min |
220℃/10kg | ASTM D1238/ISO 1133 | | g/10min |
吸水率 23℃/24H | | ASTM D570/ISO 62 | | % |
热性能 | 热变形温度 | 退火 | ASTM D648/ISO 75 | | ℃(℉) |
未退火 | ASTM D648/ISO 75 | | ℃(℉) |
维卡软化点 | | ASTM D1525/ISO R306 | | ℃(℉) |
熔点 | | - | | ℃(℉) |
燃烧性(率) | | UL94 | 1/16"HB | |
线性膨胀系数 | | ASTM D696/ISO 11359 | | mm/mm.℃ |
加工条件 | 干燥条件 | | | | |
加工温度 | 射嘴 | | | ℃ |
料筒前段 | | | ℃ |
料筒中段 | | | ℃ |
料筒后段 | | | ℃ |
熔体温度 | | | | ℃ |
模具温度 | | | | ℃ |
压力 | 注塑压力 | | | Mpa |
保压压力 | | | Mpa |
背压 | | | Mpa |
螺杆转速 | | | | rpm |
其他 | 备注 | 高耐冲击 |
颜色 | 奶白 |
特性 | 油漆桶 |
用途 | |