PropertyTest ConditionUnitStandardValue
| drying according to specifications | annealed | - |
Mechanical properties (23 °C/50 % r. h.) |
![campus image](http://tpe-u.com/_tc_bms_images_nc/xsl/campus.gif) | shore hardness, method A | | - | ISO 868 | | 97 | |
![campus image](http://tpe-u.com/_tc_bms_images_nc/xsl/campus.gif) | shore hardness, method D | | - | ISO 868 | | 57 | |
| Ultimate tensile strength | 200 mm/min | MPa | DIN 53504 | | 55,4 | |
| Strain at break | 200 mm/min | % | DIN 53504 | | 381 | |
| Stress at 10 % strain | 200 mm/min | MPa | DIN 53504 | | 13,5 | |
| Stress at 50 % strain | 200 mm/min | MPa | DIN 53504 | | 20,4 | |
| Stress at 100 % strain | 200 mm/min | MPa | DIN 53504 | | 23,6 | |
| Stress at 300 % strain | 200 mm/min | MPa | DIN 53504 | | 42,2 | |
![campus image](http://tpe-u.com/_tc_bms_images_nc/xsl/campus.gif) | Compression set | 24 h; 70 °C | % | ISO 815 | | 46 | |
![campus image](http://tpe-u.com/_tc_bms_images_nc/xsl/campus.gif) | Compression set | 72 h; 23 °C | % | ISO 815 | | 24 | |
![campus image](http://tpe-u.com/_tc_bms_images_nc/xsl/campus.gif) | Abrasion resistance | | mm³ | ISO 4649 | | 18 | |
| Impact resilience | | % | ISO 4662 | | 35 | |
| Tear propagation resistance | 500 mm/min | kN/m | ISO 34-1 | | 160 | |
Thermal properties |
| Tensile storage modulus | -20 °C | MPa | ISO 6721-1,-4 | | 2435 | |
| Tensile storage modulus | 20 °C | MPa | ISO 6721-1,-4 | | 586 | |
| Tensile storage modulus | 60 °C | MPa | ISO 6721-1,-4 | | 181 | |
Other properties (23 °C) |
![campus image](http://tpe-u.com/_tc_bms_images_nc/xsl/campus.gif) | Density | | kg/m³ | ISO 1183-1 | | | 1230 |
Molding conditions |
| Injection molding-Melt temperature | | °C | - | 220 - 240 | | |
| Injection molding-Mold temperature | | °C | - | | | 20 - 40 |
| Maximum drying temperature | | °C | - | | | 110 |