①原料描述部分
规格级别: |
注塑级 |
外观颜色: |
--- |
用途概述: |
一般用途,(一般家用制品,薄壁制品,) |
备注说明: |
--- |
②原料技术数据
性能项目 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
基本性能 |
熔体流动速率 |
--- |
ASTM D-1238 |
14 |
g/10min |
密度 |
--- |
ASTM D-792 |
0.90 |
g/cm3 |
吸水率 |
--- |
ASTM D-570 |
>0.01 |
% |
机械性能 |
线型成型收缩率 |
--- |
KPIC Method |
1.0-2.0 |
% |
拉伸强度 |
--- |
ASTM D-638 |
360 |
kgf/cm2 |
断裂伸张率 |
--- |
ASTM D-638 |
<500 |
% |
挠曲模量 |
--- |
ASTM D-790 |
17,000 |
kgf/cm2 |
洛氏硬度 |
--- |
ASTM D-785 |
102 |
scRale |
冲击强度 |
带缺口 |
ASTM D-256 |
4 |
kgf.cm/cm |
绝缘强度 |
--- |
ASTM D-149 |
40 |
KV/mm |
电气性能 |
损耗因素 |
--- |
ASTM D-150 |
2 |
10-4 |
体积电阻率 |
--- |
ASTM D-257 |
1 |
1017ohm.cm |
介电常数 |
--- |
ASTM D-150 |
2.3 |
--- |
耐电弧性 |
--- |
ASTM D-495 |
130 |
sec. |
热 性 能 |
热变形温度 |
--- |
ASTM D-648 |
110 |
℃ |
线性膨胀系数 |
--- |
ASTM D-696 |
11 |
10-5cm/cm℃ |
比热容 |
--- |
KPIC Method |
0.46 |
cal/g℃ |
热传导 |
--- |
KPIC Method |
3 |
10-4calcm/cmsec,℃ |
熔点 |
--- |
ASTM D-3418 |
165 |
℃ |
维卡软化点 |
--- |
ASTM D-1525 |
153 |
℃ | | |