供应高碳铬不锈)轴承钢9Cr18Mo 化学成分 询价
| 材料名称:(高碳铬不锈)轴承钢 |
|
|
|
|
|
|
| 牌号:9Cr18Mo |
|
|
|
|
|
|
|
| 标准:GB/T 3086-1982 |
|
|
|
|
|
|
|
●化学成份: |
|
|
|
|
|
|
|
碳 C : 0.95~1.10 |
|
|
|
|
|
|
|
| 硅 Si:≤0.80 |
|
|
|
|
|
|
|
| 锰 Mn:≤0.80 |
|
|
|
|
|
|
|
| 硫 S :≤0.030 |
|
|
|
|
|
|
|
| 磷 P :≤0.035 |
|
|
|
|
|
|
|
铬 Cr: 16.0~18.0(允许偏差:±0.15) |
|
|
|
|
|
|
| 镍 Ni:允许残余含量≤0.30 |
|
|
|
|
|
|
| 铜 Cu:允许残余含量≤0.25 |
|
|
|
|
|
|
钼 Mo: 0.40~0.70(允许偏差:±0.03) |
|
|
|
|
|
|
| 注:允许残余含量Ni+Cu≤0.50 |
|
|
|
|
|
|
●力学性能: |
|
|
|
|
|
|
|
| 抗拉强度 σb (MPa):直径≤16时,588(60)~784(80) |
|
|
|
|
|
| 硬度 :直径>16时,197~241HB,压痕直径为4.3~3.9 |
|
|
|
|
|
●热处理规范及金相组织: |
|
|
|
|
|
|
●交货状态:以热轧(锻制)退火(RT)、冷拉退火(LT)和冷拉磨光(LM)状态交货。交货状态应在合同中注明。 |