超高耐热PEI基础创新塑胶(美国)2100传感器真空泵叶轮
产品参数
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 |
| 熔体流动速率 | | ASTM D-1238 | 6.3 | g/10min |
| 吸水率 | 平衡 73H | ASTM D-570 | 1.20 | % |
| 吸水率 | 24小时,73H | ASTM D-570 | 0.210 | % |
| 模具收缩率 | | ASTM D-955 | 5-6 | in/inE-3 |
| 固体比重 | | ASTM D-792 | 1.34 |
| 挠曲模量 | | ASTM D-790 | 650000 | Psi |
| IZOD无缺口冲击强度 | | ASTM D-4812 | 9.0 | ft-lb/in |
| 断裂抗拉伸伸长 | | ASTM D-638 | 6.0 | % |
| 屈服抗拉伸长 | | ASTM D-638 | 5.0 | % |
| 屈服抗拉强度 | | ASTM D-638 | 16600 | Psi |
| 洛氏硬度 | | ASTM D-785 | 114 | Psi |
| IZOD缺口冲击强度 | | ASTM D-256 | 1.1 | ft-lb/in |
| 屈服挠曲强度 | | ASTM D-790 | 29000 | Psi |
| 损耗因数 | 1KHz | ASTM D-150 | 0.0014 |
| 介电常数 | 1KHz | ASTM D-150 | 3.50 |
| 介电强度 | 62mils | ASTM D-149 | 700 | V/mil |
| 体积电阻率 | | ASTM D-257 | 11017 | .cm |
| 燃烧性 | | UL 94 | V-0 | class |
| 线膨胀系数(flow) | | ASTM E-831 | 1105 | E-5/in/inH |
| 线膨胀系数(xflow) | | ASTM E-831 | - | E-5/in/inH |
| 热变形温度 | 66Psi | ASTM D-648 | 410 | H |
| 维卡软化点 | | ASTM D-1525 | 434 | H |
| 热指数(电性能) | | UL746B | 170 | ℃ |
| 热指数(机械冲击性能) | | UL746B | 170 | ℃ |
| 热指数(非机械性能) | | UL746B | 170 | ℃ |
| 热变形温度 | 264Psi | ASTM D-648 | 405 | H |