产品参数
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 |
物理性能 | 密度 | | ASTM D1505 | 1.30 | g/cm3; |
机械性能 | 摩擦系数 | 与金属 - 动态 | ASTM D1894 | 0.20 | |
薄膜 | 割线模量 | MD | ASTM D882 | 1720 | MPa |
| MD | ASTM D882 | 1760 | MPa |
抗张强度 | MD: 屈服 | ASTM D882 | 35.2 | MPa |
| TD: 屈服 | ASTM D882 | 27.6 | MPa |
| MD: 断裂 | ASTM D882 | 40.7 | MPa |
| TD: 断裂 | ASTM D882 | 41.4 | MPa |
伸长率 | MD: 断裂 | ASTM D882 | 440 | % |
| TD: 断裂 | ASTM D882 | 450 | % |
氧气传输速率 | 25 µm | ASTM D3985 | 190 | cm3;/m2;/24 hr |
水气透过率 | | ASTM F1249 | 47 | g/m2;/24 hr |
Elmendorf Tear Strength | MD | ASTM D1922 | 8.1 | kN/m |
| TD | ASTM D1922 | 8.5 | kN/m |
Graves Tear | MD, Unnotched | ASTM D1004 | 232.8 | kN/m |
| TD, unnotched | ASTM D1004 | 219.3 | kN/m |
Spencer Impact | | ASTM D3420 | 53.4 | J/cm |
热封强度 | 107°C | | 24 | g/2.5 cm |
| 121°C | | 2500 | g/2.5 cm |
| 135°C | | 2300 | g/2.5 cm |
| 149°C | | 3000 | g/2.5 cm |
热性能 | 玻璃转化温度 | DSC | ASTM D3418 | 75.0 | °C |
熔融温度 | | ASTM D3418 | 255 | °C |
PET(聚对苯二甲酸乙 二醇酯#聚酯)PT 4274美国杜邦 电话 13355973795 秦先生用途:其它
特性备注:保香防潮良好的热封性 食品接触的合规性粘度,高阻隔树脂 阻氧
重要参数:密度:1.3 g/cm3拉伸强度:35.2 MPa断裂伸长率:440 %