POM/美国杜邦/500P物性表:
性能项目 | 测试条件 | 测试方法 | 数值/描述 | 单位 |
机械性能 | 拉伸强度(引张强度) | | ASTM D638/ISO 527 | 70 | kg/cm²(MPa)[Lb/in2] |
断裂伸长率 | | ASTM D638/ISO 527 | | % |
拉伸模量 | | ASTM D638/ISO 527 | | kg/cm²(MPa)[Lb/in2] |
拉伸屈服伸长率(延伸率) | | ASTM D638/ISO 527 | 40 | % |
拉伸断裂伸长率(延伸率) | | ASTM D638/ISO 527 | 30 | % |
弯曲模量(弯曲弹性率) | | ASTM D790/ISO 178 | 2900 | kg/cm²(MPa)[Lb/in2] |
弯曲强度 | | ASTM D790/ISO 178 | 80 | kg/cm²(MPa)[Lb/in2] |
洛氏硬度 | | ASTM D785 | R-120 | |
IZOD 缺口冲击强度 | 1/4" 23℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
1/4" -30℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
1/8" 23℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
1/8" -30℃ | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
Charpy冲击强度 | 23℃ (缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
-30℃(缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
23℃(无缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
-30℃(无缺口) | ASTM D256/ISO 179 | | kg·cm/cm(J/M)ft·lb/in |
物性性能 | 比重(密度) | | ASTM D792/ISO 1183 | | |
成型收缩率 | | ASTM D955 | 1420 | % |
熔融指数(流动系数) | 200℃/5kg | ASTM D1238/ISO 1133 | | g/10min |
220℃/10kg | ASTM D1238/ISO 1133 | | g/10min |
吸水率 23℃/24H | | ASTM D570/ISO 62 | | % |
POM/美国杜邦/500P注塑模工艺条件:
干燥处理:如果材料储存在干燥环境中,通常不需要干燥处理。
熔化温度:均聚物材料为190~230℃;共聚物材料为190~210℃。
模具温度:80~105℃。为了减小成型后收缩率可选用高一些的模具温度。
注射压力:700~1200bar
注射速度:中等或偏高的注射速度。
流道和浇口:可以使用任何类型的浇口。如果使用隧道形浇口,则最好使用较短的类型。对于均聚物材料建议使用热注嘴流道。对于共聚物材料既可使用内部的热流道也可使用外部热流道。
POM/美国杜邦/500P型号:![POM杜邦](http://i01.c.aliimg.com/img/ibank/2013/473/246/1090642374_377408383.jpg)
Delrin®100 BK602
高粘度缩醛均聚物
Delrin®100 NC010
高粘度缩醛均聚物
Delrin®100AF
20%甲醛均聚物型Teflon®PTFE纤维
聚甲醛®100AL NC010
润滑,高粘度缩醛均聚物
Delrin®聚100KM NC000
聚甲醛均聚物的Kevlar®芳纶树脂杰出的耐磨性
聚甲醛®100P BK602
高粘度缩醛均聚物
聚甲醛®100P NC010
高粘度缩醛均聚物
聚甲醛®100PE BK602
高粘度聚甲醛均聚物,排放量非常低
聚甲醛®100PE NC010
高粘度聚甲醛均聚物,排放量非常低
'