粘土砖理化指标 Physical and chemical of fireclay brick
项 目 Item |
指 标 Index |
N-1 |
N-2a |
N-2b |
N-3a |
N-3b |
N-4 |
N-5 |
N-6 |
Al2O3 % 不小于 |
42 |
42 |
42 |
40 |
40 |
36 |
36 |
36 |
Fe2O3 % 不大于 |
1.7 |
1.7 |
1.7 |
1.8 |
1.8 |
2 |
2 |
2 |
耐火度,℃ Refractoriness |
≥1750 |
≥1730 |
≥1730 |
≥1710 |
≥1710 |
≥1690 |
≥1670 |
≥1580 |
0.2Mpa荷重软化开度,℃
Refractoriness under load |
≥1400 |
≥1350 |
|
≥1320 |
|
≥1300 |
|
|
重烧线变化率,﹪
Reheating linear change |
1400℃,2h |
+0.1
-0.4 |
+0.1
-0.5 |
+0.2
-0.5 |
|
|
|
|
|
1350℃,2h |
|
|
|
+0.2
-0.5 |
+0.2
-0.5 |
+0.2
-0.5 |
+0.2
-0.5 |
|
显气孔率,% Apparent porosity |
≤22 |
≤24 |
≤26 |
≤24 |
≤26 |
≤24 |
≤26 |
≤28 |
常温耐压强度CCS Mpa |
≥30.0 |
≥25.0 |
≥20.0 |
≥20.0 |
≥15.0 |
≥20.0 |
≥15.0 |
≥15.0 |
粘土砖产品特点:高炉用粘土砖采用优质粘土熟料为主要原料,经高压成型,高温烧结而成,主要矿物组成为莫来石相。产品具有优良的高温物理性能和抗化学侵蚀性能,广泛应用于中小高炉炉衬的各个部位。
欢迎有意客户来电咨询