| 低气孔粘土砖 | 二级高铝砖 | 硅线石砖 | 莫来石砖 | 刚玉莫来石砖 |
XND-45 | XLZ-55 | XGC-A | XGC-B | XMS-70 | XMS-80 | XMS-85 |
Al2O3≥% | 45 | 55 | 60 | 65 | 70 | 80 | 85 |
SiO2≤% | | | 38 | 33 | 28 | 18 | 14 |
常温抗压强度 ≥MPa | 45 | 45 | 75 | 75 | 90 | 120 | 90 |
体积密度 ≥g/cm3 | 2.3 | 2.4 | 2.4 | 2.45 | 2.55 | 2.6 | 2.8 |
0.2MPa荷重软化温度T0.6≥℃ | 1400 | 1420 | 1550 | 1600 | 1650 | 1650 | 1650 |
显气孔率 | 16 | 22 | 19 | 19 | 18 | 18 | 18 |
| 莫来石砖 | 合成莫来石砖 | 刚玉莫来石砖 | 电熔再结合莫来石砖 | 烧结锆刚玉砖 | 锆莫来石砖 |
XMS-70 | XMS-80 | XCM-85 | XFM-75 | XAZ-33 | XMZ-30 | XMZ-22 | XMZ-15 |
Al2O3≥% | 70 | 80 | 85 | 75 | 60 | 50 | 55 | 62 |
SiO2≤% | 28 | 18 | 14 | 23 | | | | |
Fe2O3≤% | 0.5 | 0.4 | 0.5 | 0.2 | 0.30 | 0.5 | 0.5 | 0.5 |
ZrO2≥% | | | | | 33 | 30 | 22 | 15 |
显气孔率 | 18 | 16 | 17 | 16 | 18 | 18 | 18 | 18 |
体积密度≥g/cm3 | 2.55 | 2.70 | 2.70 | 2.70 | 3.5 | 2.95 | 2.85 | 2.70 |
常温耐压≥MPa | 100 | 120 | 100 | 120 | 80 | 100 | 65 | 70 |
0.2MPa荷重软化(T0.6℃)≥ | 1650 | 1650 | 1650 | 1700 | 1680 | 1650 | 1600 | 1650 |
使用部位:莫来石砖用于玻璃熔窑上部结构,料道砖、盖板,加工窑炉上部结构,E-玻璃熔窑碹砖。锆莫来石砖具有良好的抗碱蒸汽、抗热震能力,主要用于玻璃窑火焰空间,蓄热室砖以及上部格子砖,也可做铺底亚层和料道砖。