适用于焊接19 Cr 10 Ni牌号钢种的超低碳含量不锈钢焊条。其也适用于焊接成分类似的稳定化不锈钢,母材需要满足足够抗蠕变性时除外。
Typical Tensile Properties
| As welded |
| Elongation | Tensile Strength | Yield Strength | 保护气体 |
| 45 % | 580 MPa | 430 MPa | ISO |
| - | - | - | AWS |
夏比V型缺口冲击性能| As welded |
| Impact Value | Testing Temperature | 保护气体 |
| 70 J | 20 °C | ISO |
| 49 J | -60 °C | ISO |
焊缝金属分析| Mn |
| Mn | C | Si | Ferrite FN | Ni | N | Cr |
| 0.7 % | - | - | - | - | - | - |
| C |
| Mn | C | Si | Ferrite FN | Ni | N | Cr |
| - | 0.03 % | - | - | - | - | - |
| Si |
| Mn | C | Si | Ferrite FN | Ni | N | Cr |
| - | - | 0.9 % | - | - | - | - |
| Ferrite FN |
| Mn | C | Si | Ferrite FN | Ni | N | Cr |
| - | - | - | 5 % | - | - | - |
| Ni |
| Mn | C | Si | Ferrite FN | Ni | N | Cr |
| - | - | - | - | 10.0 % | - | - |
| Cr |
| Mn | C | Si | Ferrite FN | Ni | N | Cr |
| - | - | - | - | - | - | 19.3 % |
熔敷数据| Fusion time per electrode at 90% I max | kg weld metal/kg electrodes | Number of electrodes/kg weld metal | 安培 | 熔敷率 | 电压 V | 直径 |
| 24 sec | 0.55 kg | 240 | 35-45 A | 0.6 kg/h | 27 V | 1.6 x 300 mm |
| 29 sec | 0.55 kg | 160 | 35-65 A | 0.8 kg/h | 29 V | 2.0 x 300 mm |
| 36 sec | 0.55 kg | 99 | 50-90 A | 1.1 kg/h | 31 V | 2.5 x 300 mm |
| 54 sec | 0.60 kg | 49 | 70-130 A | 1.4 kg/h | 31 V | 3.2 x 350 mm |
| 60 sec | 0.60 kg | 33 | 90-180 A | 2.0 kg/h | 32 V | 4.0 x 350 mm |
| 60 sec | 0.60 kg | 20 | 140-250 A | 3.0 kg/h | 33 V | 5.0 x 350 mm
|