Shield-Bright 309LMo X-tra was developed for the welding of stainless steels to carbon or low alloy steels. For thick sections it is often preferable that the non-stainless steel should be buttered with a layer of Shield-Bright 309L X-tra and the joint made with Shield-Bright 316L X-tra or 308L X-tra. It was also developed for the first layer cladding of carbon and low alloy steels prior to subsequent layers from Shield-Bright 316L X-tra or 317L X-tra. The service temperature of all the resulting weldments should not exceed about 700°F (370°C). Multiple layer cladding with Shield-Bright 309LMo X-tra can be used for additional corrosion resistance in some applications in the pulp and paper industry. Shield-Bright 309LMo X-tra was developed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal. It can be used with either 75% Ar / 25% CO2 or 100% CO2 gases.
Typical Tensile Properties
| As welded |
| Elongation | Tensile Strength | Yield Strength | 保护气体 |
| 30 % | 690 MPa | 550 MPa | M21 Shielding Gas |
| 33 % | 662 MPa | 527 MPa | C1 shielding Gas |
夏比V型缺口冲击性能| As welded |
| Impact Value | Testing Temperature | 保护气体 |
| 28 J | -29 °C | C1 shielding Gas |
焊缝金属分析| M21 Shielding Gas |
| IMPERIAL_M21 Shielding Gas | IMPERIAL_C1 shielding Gas |
| 2.50 % | - |
| C1 shielding Gas |
| IMPERIAL_M21 Shielding Gas | IMPERIAL_C1 shielding Gas |
| - | 2.30 % |
熔敷数据| 安培 | 熔敷率 | 电压 V | 直径 | 送丝速度 |
| 150-250 A | 2.5-7.0 kg/h | 25-32 V | 1.2 mm | 8.0-16.0 m/min
|