Brilliant 2594 T-1 AP 设计用于双相不锈钢的全焊位焊接以及低合金钢与双相不锈钢的焊接。该合金可产生喷射状电弧转移,焊渣清理方便,可通过多种参数进行焊接。AWS 类别 A5.22 E2594T1-X。
Typical Tensile Properties
| Elongation | Tensile Strength | Yield Strength | 保护气体 |
| 25 % | 126 ksi | 99 ksi | 100% CO2 |
夏比V型缺口冲击性能| Condition | Impact Value | 测试温度(焊态) |
| As Welded | 33 ft-lb | -40 °C |
焊缝金属分析| Mn |
| Mn | Mo | C | Si | Ni | N | Cr | Fe |
| 0.7 % | - | - | - | - | - | - | - |
| Mo |
| Mn | Mo | C | Si | Ni | N | Cr | Fe |
| - | 4.0 % | - | - | - | - | - | - |
| C |
| Mn | Mo | C | Si | Ni | N | Cr | Fe |
| - | - | 0.03 % | - | - | - | - | - |
| Si |
| Mn | Mo | C | Si | Ni | N | Cr | Fe |
| - | - | - | 0.6 % | - | - | - | - |
| Ni |
| Mn | Mo | C | Si | Ni | N | Cr | Fe |
| - | - | - | - | 8.9 % | - | - | - |
| Cr |
| Mn | Mo | C | Si | Ni | N | Cr | Fe |
| - | - | - | - | - | - | 24.7 % | - |
| Fe |
| Mn | Mo | C | Si | Ni | N | Cr | Fe |
| - | - | - | - | - | - | - | BAL % |
熔敷数据| Deposition Type | TTW距离 | TTW距离(导电嘴到母材距离) | 保护气体 | 安培 | 电压 V | 直径 | 送丝速度 |
| Full Range | 13 mm | 1/2 in. | 75% Ar - 25% CO2 | 130-220 A | 24-27 V | .045 in. | 227-565 in./min |
| Full Range | 13 mm | 1/2 in. | 75% Ar - 25% CO2 | 170-300 A | 25-28 V | 1.6 mm | 155-320 in./min |