适用于诸如容器、管道及海洋工程应用中最小屈服强度低于470 Mpa低合金及低温钢种GMAW焊接的镀铜镍合金(2,4% Ni)实芯焊丝。该焊丝在-60°C条件下具有良好的冲击韧性。
Typical Tensile Properties| AWS Ar/1-5O2 (M13) Stress relieved |
| Elongation | Stress Relieved Temperature | Stress Relieved Testing Time | Tensile Strength | Yield Strength |
| 29 % | 620 °C | 1 hr | 630 MPa | 540 MPa |
| EN Ar/20CO2 (M21) As welded |
| Elongation | Stress Relieved Temperature | Stress Relieved Testing Time | Tensile Strength | Yield Strength |
| 28 % | - | - | 630 MPa | 540 MPa |
夏比V型缺口冲击性能| AWS Ar/1-5O2 (M13) Stress relieved |
| Impact Value | Stress Relieved Testing Temp | Stress Relieved Testing Time | Testing Temperature |
| 162 J | 620 °C | 1 hr | 0 °C |
| 168 J | 620 °C | 1 hr | -29 °C |
| 131 J | 620 °C | 1 hr | -62 °C |
| EN Ar/20CO2 (M21) As welded |
| Impact Value | Stress Relieved Testing Temp | Stress Relieved Testing Time | Testing Temperature |
| 130 J | - | - | 0 °C |
| 100 J | - | - | -40 °C |
| - | - | - | -50 °C |
| 60 J | - | - | -60 °C |
焊缝金属分析| Mn |
| Mn | C | Si | Ni | Cr |
| 1.04 % | - | - | - | - |
| C |
| Mn | C | Si | Ni | Cr |
| - | 0.08 % | - | - | - |
| Si |
| Mn | C | Si | Ni | Cr |
| - | - | 0.53 % | - | - |
| Ni |
| Mn | C | Si | Ni | Cr |
| - | - | - | 2.36 % | - |
| Cr |
| Mn | C | Si | Ni | Cr |
| - | - | - | - | 0.03 % |
熔敷数据| 安培 | 熔敷率 | 电压 V | 直径 | 送丝速度 |
| 40-170 A | 0,4-2,6 kg/h | 16-22 V | 0.8 mm | 2-10,8 m/min |
| 80-280 A | 1-5,4 kg/h | 18-28 V | 1.0 mm | 2,7-14,7 m/min |
| 120-350 A | 1,5-6,6 kg/h | 20-33 V | 1.2 mm | 2,7-12,4 m/min |