适用于高温钢及炼油厂等非临氢作业用钢材GMAW焊接的镀铜低合金铬钼(9% Cr, 1% Mo)实芯焊丝。
Typical Tensile Properties
| EN 80Ar/20CO2 (M21) Stress relieved |
| Elongation | Stress Relieved Temperature | Stress Relieved Testing Time | Tensile Strength | Yield Strength |
| 23 % | 760 °C | 2 hr | 620 MPa | 536 MPa |
| AWS Ar/1-5%O2 (M13) Stress relieved |
| Elongation | Stress Relieved Temperature | Stress Relieved Testing Time | Tensile Strength | Yield Strength |
| 22 % | 745 °C | 2 hr | 680 MPa | 523 MPa |
夏比V型缺口冲击性能| EN 80Ar/20CO2 (M21) Stress relieved |
| Impact Value | Stress Relieved Testing Temp | Stress Relieved Testing Time | Testing Temperature |
| 91 J | 760 °C | 2 hr | 20 °C |
| 50 J | 760 °C | 2 hr | -20 °C |
| AWS Ar/1-5%O2 (M13) Stress relieved |
| Impact Value | Stress Relieved Testing Temp | Stress Relieved Testing Time | Testing Temperature |
| 115 J | 745 °C | 2 hr | 20 °C |
| 50 J | 745 °C | 2 hr | -20 °C |
焊缝金属分析| Mn |
| Mn | Mo | C | Si | Ni | Cr |
| 0.52 % | - | - | - | - | - |
| Mo |
| Mn | Mo | C | Si | Ni | Cr |
| - | 1.00 % | - | - | - | - |
| C |
| Mn | Mo | C | Si | Ni | Cr |
| - | - | 0.06 % | - | - | - |
| Si |
| Mn | Mo | C | Si | Ni | Cr |
| - | - | - | 0.45 % | - | - |
| Ni |
| Mn | Mo | C | Si | Ni | Cr |
| - | - | - | - | 0.23 % | - |
| Cr |
| Mn | Mo | C | Si | Ni | Cr |
| - | - | - | - | - | 8.66 % |
熔敷数据| 安培 | 熔敷率 | 电压 V | 直径 | 送丝速度 |
| 70-250 A | 0.9-3.5 kg/h | 18-26 V | 0.9 mm | 3.0-12 m/min |
| 120-350 A | 1,5-6,6 kg/h | 20-33 V | 1.2 mm | 2,7-12,4 m/min
|